NEWS

Why do some potting compounds crack after just six months, even though they’re all the same type of encapsulant?

In the field of electronic packaging, potting technology serves as a critical safeguard for core components such as power modules, sensors, IGBT power modules, and transformers. With its outstanding electrical insulation properties, chemical resistance, and superior water- and moisture-proof performance, potting compound has become the material of choice for encapsulating electronic products.

Many engineers and procurement professionals have encountered this vexing issue:

 

The sample appeared intact after potting, and passed factory‑level testing without issue. However, after just a few months of operation at the customer’s site, the encapsulant developed fine cracks, delamination, and peeling.

 

Many people assume it’s simply due to poor adhesive quality, but numerous failure cases demonstrate that cracks that only become apparent after six months are usually not caused by the adhesive failing on the spot; rather, they are… The long-term accumulation of stress and the resulting fatigue failure give rise to problems that arise from the combined effects of material properties, structural design, manufacturing processes, and service environment.

 

Let’s first distinguish between two failure modes that are easily confused, so we can pinpoint the right approach when troubleshooting:

 

Cleavage of the bulk colloid (cohesive failure): Cracks propagate from within the colloid, causing the adhesive layer itself to fracture; the root cause is… Insufficient adhesive toughness, excessive thermal stress, and internal bubble defects;

 

Interface debonding (often mistakenly referred to as cracking): Gaps appear at the interfaces between the adhesive and the housing, the PCB, and the components; the adhesive itself remains intact. The root cause is insufficient adhesion and contamination on the substrate surfaces.


 

I. The core factors of formulation and environmental conditions that induce intrinsic cracking:

 

1. Powder dispersibility issues

 

The particle size and distribution of alumina thermal‑conductive powder directly affect the performance of potting compounds. Excessive particle size or uneven particle size distribution can lead to localized stress concentrations, which in turn may cause cracking.

 

When the filler content is too high or unevenly dispersed, weak spots are likely to form within the potting compound, increasing the risk of cracking.

 

Solution: Select modified alumina powders with particle-size matching and uniform particle-size distribution; control the filler loading ratio, optimize the stirring and dispersion process, and, when necessary, use appropriate dispersants to minimize filler agglomeration and prevent localized stress concentrations.

2. Crosslinking Relationship Issues

 

Unreasonable process parameters, such as the component ratios in the formulation, stirring speed, and mixing time, can lead to an uneven crosslinking structure and reduce the material’s toughness.

 

When the filler exhibits poor compatibility with the matrix, interfacial adhesion is insufficient, making the interface prone to cracking under stress.

 

Solution: Formulated according to weight ratios, the curing components are used as a matched pair; crosslink density is adjusted based on operating conditions, and an appropriate curing profile is selected to ensure uniform and stable crosslinking. The Hinnel potting compound’s curing system has been optimized and can be tailored to achieve an appropriate crosslinking density based on the customer’s operating conditions.

 

3. Curing Shrinkage Issues

 

During the curing process, the encapsulant releases heat, leading to volumetric shrinkage; if the resulting shrinkage stresses exceed the material’s strength limit, cracking may occur.

 

Excessively rapid curing or an overly steep temperature gradient can exacerbate non-uniform shrinkage, increasing the risk of cracking.

 

Solution: Employ a low-shrinkage formulation system and optimize the filler loading ratio to reduce overall curing shrinkage; thick adhesive layer. A layered potting and stepwise heating‑curing process is employed, with strict control of the heating rate to prevent rapid curing over short periods. Allow the shrinkage stress to dissipate gradually, thereby preventing stress concentrations that could trigger cracking in the colloid.

 

4. External Environmental Factors

 

Harsh environmental conditions, such as drastic temperature fluctuations, high humidity, or mechanical vibration, can accelerate material aging or induce stress concentrations, thereby leading to cracking.

 

Prolonged thermal cycling or exposure to chemically corrosive environments may degrade material properties and reduce crack‑resistance.

 

Solution : Select components based on operating conditions and conduct high‑ and low‑temperature tests as well as the Double 85 reliability test in advance. For vibration‑prone applications, use elastomeric gaskets and adopt sealed housings with optimized structural design to mitigate environmental stress‑induced deformation. Hinnel’s entire line of potting compounds undergoes high- and low-temperature cycling and double 85 humidity‑heat aging tests before leaving the factory, making them suitable for demanding operating conditions.

 

II. Causes of Interfacial Debonding in Potting Adhesives:

 

Cracks appear at the interfaces between the potting compound and the housing, the PCB, and the components; the compound itself shows no signs of damage or cracking. The primary causes are residual contaminants—such as oil, dust, or release agents—on the substrate surface, or insufficient adhesion of the adhesive to the substrate, which prevents the formation of a stable bonding layer. Under thermal cycling and mechanical stress, these interfaces gradually delaminate.

 

Solution: Prior to potting, perform degreasing and dust‑removal cleaning on the housing, PCB, and component surfaces. For substrates that are difficult to bond, apply a dedicated primer to enhance interfacial adhesion, while maintaining rigorous process control to prevent secondary contamination of the substrate.


 

III. How to Choose Adhesives for Different Electronic Products?

 

Motor stator potting

 

Servo motors / frameless torque stators, new‑energy drive motor stators, conventional brushless stators, micro‑motor stators (for small household appliances), etc.; these components generate significant heat, and their high‑speed, alternating‑vibration coils are prone to loosening.

 

Recommended to follow:

 

✅Temperature Resistance Grade

✅Dielectric withstand voltage

✅Vibration-resistant and anti-loosening

✅Thermal conductivity

✅Viscosity-adapted process

✅Curing efficiency

 

Recommended adhesive: Hinnel HN6220D, HN6225D, HN6223D, HN6228D, HN6330D High-thermal-conductivity epoxy potting compound.

Potting of smart water meters

 

Smart water meters are prone to corrosion of their circuit boards—and subsequent failure—due to prolonged exposure to humid condensation, outdoor temperature fluctuations, and moisture ingress.

 

Recommended to follow:

 

✅ Hydrolysis-resistant

✅Insulation and waterproofing

✅ Resistant to high and low temperatures

✅Low stress

✅Anti-aging

✅Flame-retardant

 

Recommended adhesive: Hinnel epoxy potting compound, for example: HNEP6220/HNEP6230.

 

Controller potting

 

During operation, the controller generates significant heat, experiences thermal cycling, and is subjected to continuous vibration, making it susceptible to component damage and short circuits caused by moisture and dust.

 

Recommended to follow:

 

✅Thermal insulation

✅ Resistant to thermal shock

✅Low stress

✅Flame-retardant

✅Vibration-resistant

 

Recommended adhesives: Hinnel Organosilicon potting compound, Polyurethane potting compound, For example: HNSIL8730/ HNPU550.

 

IV. What can Hinnel New Materials offer?

 

Hinnel New Materials has been specializing in electronic adhesives for many years, supplying high-thermal-conductivity epoxy, silicone, polyurethane, and other electronic potting compounds. We offer sample testing, failure analysis, operating-condition selection, and curing‑process guidance; customize formulations on demand; and provide supporting documentation such as TDS and RoHS compliance reports. We address challenges related to potting‑induced cracking and thermal‑insulation performance in products like motors, smart water meters, PCBs, and controllers.

 

Note: Some content is sourced from the internet; please contact us for removal if there are any infringements.

 

 

linnel

 

°   Send an email to sales@hinnel.com Email box ;

°   Whatsapp:  86- 18301723907.